  • Effect of Surface Pre-treatments and Ageing on the Adhesive Strength of Polymer Joints
  • Kaner S, Sekercioglu T
  • 표면처리와 에이징이 고분자의 접착강도에 미치는 영향
  • Kaner S, Sekercioglu T
References
  • 1. Sekercioglu T, Kaner S, Muhendis ve Makine, 648, 37 (2014)
  •  
  • 2. Softal Electronic Gmbh, Corona pre-treatment to obtain wettability and adhesion, http://www.softal.de/, Report Nr: 102E, 2016 (accessed 12.06.16).
  •  
  • 3. Ebnessajjad S, Surface Treatment of Materials for Adhesion Bonding, 2nd ed., William Andrew - Elsevier, New York, 2014.
  •  
  • 4. Chan CM, Ko TM, Hiraoka H, Polymer Surface Modification by Plasma and Photos, Surface Science Reports 24, 1996.
  •  
  • 5. Ku SG, Park BS, Kim DW, Kim KS, Kim YC, Polym. Korea, 40(5), 671 (2016)
  •  
  • 6. Anagreh N, Dorn L, Bilke-Krause C, Int. J. Adhes. Adhes., 28, 16 (2007)
  •  
  • 7. Molitor P, Barron V, Young T, Int. J. Adhes. Adhes., 21, 129 (2001)
  •  
  • 8. Dobbi A, Bouabdallah A, Bouchama M, Meghoufel FZ, Hassini N, Polym. Eng. Sci., 52(11), 2304 (2012)
  •  
  • 9. Iqbal HMS, Bhowmik S, Benedictus R, Surface modification of high performance polymers by atmospheric pressure plasma and failure mechanism of adhesive bonded joints, Faculty of Aerospace Engineering, Delft University of Technology, Netherlands, 2010.
  •  
  • 10. Ersoy A, Kuntman A, Polimerik yalitkanlarda yuzey ozelliklerinin temas acisi ile incelenmesi, Elektrik-Elektronik-Bilgisayar Muhendisligi Sempozyumu (ELECO2008), Bursa, Turkiye, pp. 107-111 (2008).
  •  
  • 11. Zhou S, Hawley MC, Compos. Struct., 61, 303 (2003)
  •  
  • 12. Kinloch AJ, Adhesion and Adhesives, Science and Technology, Chapman and Hall, London, 1987.
  •  
  • 13. Kraus E, Orf L, Baudrit B, Heidemeyer P, Bastian M, Bonenberger R, Starostina I, Stoyanov O, Appl. Surf. Sci., 371(-), 365 (2016)
  •  
  • 14. Moghadamzadeh H, Rahimi H, Asaddlahzadeh M, Hemmati AR, Int. J. Adhes. Adhes., 31, 816 (2011)
  •  
  • 15. Han SH, Kim BJ, Park JS, Thin Solid Films, 572(-), 73 (2014)
  •  
  • 16. Brewis DM, Mathieson I, Wolfensberger M, Int. J. Adhes. Adhes., 15, 87 (1995)
  •  
  • 17. Encinas N, Diaz-Benito B, Abenojar J, Martinez MA, Surf. Coat. Technol., 205, 396 (2010)
  •  
  • 18. Encinas N, Abenojar J, Martinez MA, Int. J. Adhes. Adhes., 33, 1 (2012)
  •  
  • 19. Ku JH, Jung IH, Rhee KY, Park SJ, Compos. Part B, 45, 1282 (2013)
  •  
  • 20. Wu Y, Li J, Carlson BE, Lu P, Balogh MP, Irish NP, Mei Y, Surf. Coat. Technol., 304, 340 (2016)
  •  
  • 21. ASTM D 950-3, Standard test method for impact strength of adhesive bonds, 2011.
  •  
  • 22. Weicon Easy-Mix PE-PP 45 Technical Data Sheet, https:// www.weicon.de, (accessed 18.04.2017).
  •  
  • 23. ASTM D 6105-04, Standard practice for application of electrical discharge surface treatment of plastics for adhesive bonding, 2012.
  •  
  • 24. ASTM D 2093-03, Standard practice for preparation of surfaces of plastics prior to adhesive bonding, 2011.
  •  
  • 25. Tantec A/S, Product information for corona discharge treatment, http://www.tantec.com, (accessed 20.06.2016).
  •  
  • 26. Tantec A/S, Product information for plasma treatment treat, http:/ /www.tantec.com, (accessed 20.06.2016).
  •  
  • 27. EN 2243-5, Aerospace series - Nonmetallic material - Structural adhesives - Test method - Part 5: Ageing tests, 2011.
  •  
  • Polymer(Korea) 폴리머
  • Frequency : Bimonthly(odd)
    ISSN 0379-153X(Print)
    ISSN 2234-8077(Online)
    Abbr. Polym. Korea
  • 2023 Impact Factor : 0.4
  • Indexed in SCIE

This Article

  • 2017; 41(5): 827-834

    Published online Sep 25, 2017

  • 10.7317/pk.2017.41.5.827
  • Received on Mar 10, 2017
  • Revised on Nov 30, -0001
  • Accepted on May 7, 2017

Correspondence to

  • E-mail: